Baking wood for my next project

posted 25 Nov 2014, 22:10 by Peter Grankulla   [ updated 25 Nov 2014, 22:18 ]
I heat treated one south European and one Finnish at the same time. It is quite clear which one is better. Finnish wood has a lot of resin in it as you can see from the second image. I think we can draw some conclusions! The numbers speak for them selves too, both frequencies and weight loss. I will use some of the Finnish wood but definitely not without heat treatment. For my next one I'm going to use A & B 

European A 403 375 -6,9 %
  B 414 385 -7,0 %
Finnish C 348 318 -8,6 %
  D 333 305 -8,4 %



  