Back wood

Post date: Sep 02, 2014 10:17:15 AM

Measurements of the back wood, I observed that the speed of sound measured by 2LF dropped after sawing ribs from the wedges (3 mm)

The wood is very even and straight cut. These figures are after the heat treatment: Heat treatment jun. 23